Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.650 W/m-K @Temperature 400 °C |
4.51 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek Pyrocast AR PLUS Castable Refractory Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed... |
|||
Thermal Conductivity | 0.650 - 0.750 W/m-K @Temperature 1000 °C |
4.51 - 5.20 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 127 S Dense Refractory Castable Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value.. |
|||
Thermal Conductivity | 0.650 - 0.750 W/m-K @Temperature 1200 °C |
4.51 - 5.20 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Thermal Conductivity | 0.650 - 0.750 W/m-K @Temperature 1300 °C |
4.51 - 5.20 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Thermal Conductivity | 0.650 - 0.750 W/m-K @Temperature 1300 °C |
4.51 - 5.20 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.650 - 0.750 W/m-K @Temperature 600 °C |
4.51 - 5.20 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord.. |
|||
Thermal Conductivity | 0.650 - 0.750 W/m-K @Temperature 1300 °C |
4.51 - 5.20 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 145 CC Dense Refractory Castable Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.650 - 0.750 W/m-K @Temperature 1400 °C |
4.51 - 5.20 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast CURON 150 HR GM Dense Refractory Castable Description: Curon 150 HR GM is a gunning castable, because of its low iron content also very well suitable under reducing circumstances. In addition, this castable has a good thermal shock resistan.. |
|||
Thermal Conductivity | 0.650 W/m-K @Temperature 400 °C |
4.51 BTU-in/hr-ft²-°F @Temperature 752 °F |
parallel to thickness |
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |