Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 4.50 - 6.50 W/m-K @Temperature 600 °C |
31.2 - 45.1 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Thermal Conductivity | 4.50 W/m-K @Temperature 427 °C |
31.2 BTU-in/hr-ft²-°F @Temperature 801 °F |
parallel to thickness |
Zircar Refractory Composites RS-200 Refractory Sheet ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Thermal Conductivity | 4.50 W/m-K @Temperature 427 °C |
31.2 BTU-in/hr-ft²-°F @Temperature 801 °F |
parallel to thickness |
Zircar Refractory Composites RS-201 Refractory Sheet ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Thermal Conductivity | 4.50 W/m-K @Temperature 427 °C |
31.2 BTU-in/hr-ft²-°F @Temperature 801 °F |
parallel to thickness |
Zircar Refractory Composites RS-202 Refractory Sheet ZRCI Refractory Sheet Type RS-202 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |