Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.510 W/m-K @Temperature 427 °C |
3.54 BTU-in/hr-ft²-°F @Temperature 801 °F |
|
Pyrotek Dry Cathode Barrier Material In the presence of cryolite, Dri-Barrier Mix is designed to form a viscous layer on its surface which prevents further penetration. The freezing isotherm sustained in Dri-Barrier Mix decreases the .. |
|||
Thermal Conductivity | 0.510 W/m-K @Temperature 698 °C |
3.54 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Pyrotek Pyrocast AR LITE Castable Refractory A light weight highly insulating refractory product which offers excellent resistance to molten aluminum erosion and thermal shock.ApplicationsFor conveyance and casting of aluminum and its alloys A.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 120 Dense Refractory Castable Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 120 HS Dense Refractory Castable Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars... |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 100 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 100 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 140 Dense Refractory Castable Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this castable can be applied up to 1400°C in slightly reducing atmospheres. Up to high temperatures Curo.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 100 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 150 HS Dense Refractory Castable Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 1400 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by .. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus.. |
|||
Thermal Conductivity | 0.510 - 0.610 W/m-K @Temperature 600 °C |
3.54 - 4.23 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan.. |
|||
Thermal Conductivity | 0.510 W/m-K @Temperature 816 °C |
3.54 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-32 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |