Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 100 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 110 C Dense Refractory Castable Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 100 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 110 Dense Refractory Castable Description: Curon 110 is an easily workable castable, especially developed to cast complicated shapes. Because of its low shrinkage, this castable has less tendency to crack.Remarks: These values a.. |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 1000 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu.. |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 100 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 145 P Dense Refractory Castable Description: This material with an extreme plasticity is well suited for repair work or application as a thin layer.Remarks: These values apply to cast products.Information provided by Gouda Vuurvas.. |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 1000 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast... |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 1260 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 2300 °F |
|
Gouda Vuurvast GOLITE 135 Refractory Insulating Castable Description: Golite 135 can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning vari.. |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 100 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 100 Dense Refractory Castable Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 1600 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Zircar Ceramics ALBF Alumina Bulk Fiber Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give .. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 1600 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Zircar Ceramics ALBF-1 Alumina Bulk Fiber Type ALBF-1 Alumina Bulk Fiber is a specially cleaned alumina fiber with relatively short fiber lengths. It is suitable for use in vacuum forming of high density rigid boards & shapes, in the reinfo.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 816 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-3000 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.450 W/m-K @Temperature 1000 °C |
3.12 BTU-in/hr-ft²-°F @Temperature 1830 °F |
ASTM C182 |
BNZ Materials Color CA Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 100 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 100 C Dense Refractory Castable Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values .. |
|||
Thermal Conductivity | 0.450 - 0.550 W/m-K @Temperature 1000 °C |
3.12 - 3.82 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast FI 35-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |