Polymer Property : Thermal Conductivity = 270 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 38.9 W/m-K

@Temperature 302 °C
270 BTU-in/hr-ft²-°F

@Temperature 575 °F
Schmolz + Bickenbach Cryodur® 2312 (Brake Die) Cold Work Die Steel
Description: Cryodur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared t..
Thermal Conductivity 38.9 W/m-K

@Temperature 200 °C
270 BTU-in/hr-ft²-°F

@Temperature 392 °F
Annealed
Schmolz + Bickenbach Cryodur® 2767 Cold Work Die Steel
Description: High hardenability and toughness, highly suitable for polishing, texturing and EDM machining. We recommend the use of Cryodur® 2767 (ERS) for extreme demandsApplications: Cutlery dies,..
Thermal Conductivity 38.9 W/m-K

@Temperature 302 °C
270 BTU-in/hr-ft²-°F

@Temperature 575 °F
Schmolz + Bickenbach Formadur® 2312 (Ultra Holder) Plastic Mold Steel
Description: Formadur® 2312 is a pre-hardened single melt Extra Fine Structure (EFS) plastic mold steel and Re-sulphurized to improve machinabilityCharacteristics: Excellent machinability compared ..