Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 30.0 W/m-K @Temperature 20.0 °C |
208 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such .. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 700 °C |
208 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 500 °C |
208 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to .. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 199 °C |
208 BTU-in/hr-ft²-°F @Temperature 390 °F |
hardened to 57 HRC |
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh.. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 599 °C |
208 BTU-in/hr-ft²-°F @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 599 °C |
208 BTU-in/hr-ft²-°F @Temperature 1110 °F |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 199 °C |
208 BTU-in/hr-ft²-°F @Temperature 390 °F |
hardened to 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 399 °C |
208 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardened to 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 100 °C |
208 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 800 °C |
208 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Thermal Conductivity | 30.0 W/m-K @Temperature 204 °C |
208 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi.. |