Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.430 W/m-K @Temperature 204 °C |
2.98 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Pyrotek Dry Cathode Barrier Material In the presence of cryolite, Dri-Barrier Mix is designed to form a viscous layer on its surface which prevents further penetration. The freezing isotherm sustained in Dri-Barrier Mix decreases the .. |
|||
Thermal Conductivity | 0.430 W/m-K @Temperature 449 °C |
2.98 BTU-in/hr-ft²-°F @Temperature 840 °F |
hot face 548°C, cold face 350°C, mean - 449°C |
Pyrotek Insural® 140 Insulating Refractory Shapes for Aluminum Insural® 140 Precast Shapes are designed for the containment of molten aluminum in hot top modules (cross feeder) and trough/launder applications.AdvantagesNear zero expansion avoids gaps at the jo.. |
|||
Thermal Conductivity | 0.430 - 0.530 W/m-K @Temperature 1000 °C |
2.98 - 3.68 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar.. |
|||
Thermal Conductivity | 0.430 W/m-K @Temperature 1650 °C |
2.98 BTU-in/hr-ft²-°F @Temperature 3000 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.430 W/m-K @Temperature 1093 °C |
2.98 BTU-in/hr-ft²-°F @Temperature 1999 °F |
|
3M 615+ Fire Barrier Duct Wrap 3M Fire Barrier Duct Wrap 615+ is a flexible fire-resistant wrap consisting of an inorganic fiber blanket encapsulated with a scrim-reinforced foil. The product is 1-1/2 in. thick, 6pcf density. It .. |
|||
Thermal Conductivity | 0.430 W/m-K @Temperature 1650 °C |
2.98 BTU-in/hr-ft²-°F @Temperature 3000 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |