Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.4 W/m-K @Temperature 500 °C |
169 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
International Mold Steel Daido DRM3 Matrix High-Speed Steel This conventional grade MH88 has been improved to DRM3. High hardness and tough DRM3 with excellent hardenability is suitable for high precision cold working tools.Information provided by Internatio.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 500 °C |
169 BTU-in/hr-ft²-°F @Temperature 932 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 500 °C |
169 BTU-in/hr-ft²-°F @Temperature 932 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 24.3 W/m-K @Temperature 100 °C |
169 BTU-in/hr-ft²-°F @Temperature 212 °F |
Hardened and Tempered |
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel Properties:Hot work tool steel featuring excellent hot tensile properties, high hot wear resistance, adequate toughness and heat checking resistance, adequate toughness and heat checking; admits wat.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 500 °C |
169 BTU-in/hr-ft²-°F @Temperature 932 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 500 °C |
169 BTU-in/hr-ft²-°F @Temperature 932 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 500 °C |
169 BTU-in/hr-ft²-°F @Temperature 932 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 500 °C |
169 BTU-in/hr-ft²-°F @Temperature 932 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 300 °C |
169 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr.. |
|||
Thermal Conductivity | 24.4 W/m-K @Temperature 350 °C |
169 BTU-in/hr-ft²-°F @Temperature 662 °F |
|
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr.. |