Thermal Conductivity 21.6 W/m-K

@Temperature 600 °C
150 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 21.6 W/m-K

@Temperature 600 °C
150 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 21.6 W/m-K

@Temperature 600 °C
150 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 21.6 W/m-K

@Temperature 600 °C
150 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 21.6 W/m-K

@Temperature 600 °C
150 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 21.6 W/m-K

@Temperature 600 °C
150 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Haynes Hastelloy® C-2000® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Thermal Conductivity 21.6 W/m-K

@Temperature 538 °C
150 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Crucible Steel 303 Plus Chromium-Nickel Steel
Crucible 303 Plus is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of..
Thermal Conductivity 21.6 W/m-K

@Temperature 538 °C
150 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Crucible Steel 303 SE Chromium-Nickel Steel
Crucible 303 SE is a non-hardenable austenitic chromium-nickel steel to which selenium has been added to improve machinability and non-galling characteristics. This grade is non-magnetic in the anne..
Thermal Conductivity 21.6 W/m-K

@Temperature 538 °C
150 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Crucible Steel 347 Chromium-Nickel Steel
Crucible 347 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi..
Thermal Conductivity 21.6 W/m-K

@Temperature 538 °C
150 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Crucible Steel 348 Chromium-Nickel Steel
Crucible 348 is a non-hardenable austenitic chromium-nickel steel which are particularly adaptable for use at temperatures between 800 and 1650°F. This grade is non-magnetic in the annealed conditi..
Thermal Conductivity 21.6 W/m-K

@Temperature 538 °C
150 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Crucible Steel 304L Chromium-Nickel Steel
Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i..