Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 18.2 W/m-K @Temperature 500 °C |
126 BTU-in/hr-ft²-°F @Temperature 932 °F |
Annealed Condition |
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re.. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 300 °C |
126 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 400 °C |
126 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Carpenter 20-Mo6® Stainless Steel, Plate Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 400 °C |
126 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Carpenter 20-Mo6® Stainless Steel, Strip Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 400 °C |
126 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Carpenter 20-Mo6® Stainless Steel, Tensile Properties at 93°C Data provided by Carpenter Technology Corporation.This is an austenitic stainless steel which is resistant to corrosion in hot chloride environments with low pH. It has good resistance to pitting, .. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 200 °C |
126 BTU-in/hr-ft²-°F @Temperature 392 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Annealed Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 200 °C |
126 BTU-in/hr-ft²-°F @Temperature 392 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 200 °C |
126 BTU-in/hr-ft²-°F @Temperature 392 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 200 °C |
126 BTU-in/hr-ft²-°F @Temperature 392 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 200 °C |
126 BTU-in/hr-ft²-°F @Temperature 392 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 18.2 W/m-K @Temperature 200 °C |
126 BTU-in/hr-ft²-°F @Temperature 392 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |