Polymer Property : Thermal Conductivity = 111 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 16.0 W/m-K

@Temperature 300 °C
111 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C)
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Thermal Conductivity 16.0 W/m-K

@Temperature 300 °C
111 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicat..
Thermal Conductivity 16.0 W/m-K

@Temperature 400 °C
111 BTU-in/hr-ft²-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked
Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Thermal Conductivity 16.0 W/m-K

@Temperature 400 °C
111 BTU-in/hr-ft²-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked
Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Thermal Conductivity 16.0 W/m-K

@Temperature 400 °C
111 BTU-in/hr-ft²-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked
Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Thermal Conductivity 16.0 W/m-K

@Temperature 400 °C
111 BTU-in/hr-ft²-°F

@Temperature 752 °F
Hardened Condition
Bohler-Uddeholm BÖHLER W302 SUPERIOR® Premium H13 Tool Steel
A premium grade H13 hot work tool steel featuring:Very good toughness properties meeting the requirements of NADCA 207-97, and the superior quality levels of NADCA 207-2003Very good heat checking re..
Thermal Conductivity 16.0 W/m-K

@Temperature 20.0 °C
111 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
hardened to 50 HRC
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420
Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd..
Thermal Conductivity 16.0 W/m-K

@Temperature 100 °C
111 BTU-in/hr-ft²-°F

@Temperature 212 °F
AK Steel 321 Austenitic Stainless steel
AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 ..
Thermal Conductivity 16.0 W/m-K

@Temperature 300 °C
111 BTU-in/hr-ft²-°F

@Temperature 572 °F
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is..
Thermal Conductivity 16.0 W/m-K

@Temperature 400 °C
111 BTU-in/hr-ft²-°F

@Temperature 752 °F
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked
Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.