Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.280 W/m-K @Temperature 800 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Pyrotek B-3A REFRACTORY BOARD Pyrotek B-3A is a high density calcium silicate board specifically designed for demanding applications such as holding furnaces, launder linings and baffle plates. Its high density and superior har.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 315 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 599 °F |
|
Pyrotek ISOMAG® 175 Structural Insulation Board Isomag® 70 is a high strength insulating board suitable as an electrical insulator or a thermal barrier material in a variety of industrial applications. Its magnesia silicate based formulation pr.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 200 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Pyrotek Pyrotherm M-68 Structural Insulation Board Pyrotherm M-68 is a calcium-silicate board designed for non-ferrous applications. M-68 offers a unique combination of low shrinkage, low thermal conductivity and non-wetting properties which make i.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 300 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Pyrotek Pyrotherm M-68 Structural Insulation Board Pyrotherm M-68 is a calcium-silicate board designed for non-ferrous applications. M-68 offers a unique combination of low shrinkage, low thermal conductivity and non-wetting properties which make i.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 100 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled
(discontinued **) Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.280 - 0.360 W/m-K @Temperature 1000 °C |
1.94 - 2.50 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Thermal Conductivity | 0.280 - 0.380 W/m-K @Temperature 600 °C |
1.94 - 2.64 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Thermal Conductivity | 0.280 - 0.380 W/m-K @Temperature 100 °C |
1.94 - 2.64 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE LW Refractory Insulating Castable Description: This light weight (LW) castable can be used as a hot face material, as well as for the backlining of a dense castable or brickwork.Remarks: These values apply to cast products. Also ava.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 1650 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 3000 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 600 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials Color A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 257 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 495 °F |
|
BNZ Materials CS85 High Temperature Structural Insulation NZ manufactures a variety of non-asbestos calcium silicate structural insulations that combine high strength and excellent thermal insulating characteristics for use in a variety of heat processing,.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 427 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 801 °F |
|
BNZ Materials Marinite® A Ceramic Board for Aluminum Contact These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 538 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
BNZ Materials Marinite® A Ceramic Board for Aluminum Contact These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou.. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 815 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
3M 615+ Fire Barrier Duct Wrap 3M Fire Barrier Duct Wrap 615+ is a flexible fire-resistant wrap consisting of an inorganic fiber blanket encapsulated with a scrim-reinforced foil. The product is 1-1/2 in. thick, 6pcf density. It .. |
|||
Thermal Conductivity | 0.280 W/m-K @Temperature 1650 °C |
1.94 BTU-in/hr-ft²-°F @Temperature 3000 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ALCAA Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |