Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.125 W/m-K @Temperature 218 °C |
0.864 BTU-in/hr-ft²-°F @Temperature 425 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Thermal Conductivity | 0.125 W/m-K @Temperature 100 °C |
0.864 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ChevronTexaco 46 Heat Transfer Oil FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont.. |
|||
Thermal Conductivity | 0.125 W/m-K @Temperature 100 °C |
0.864 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |
|||
Thermal Conductivity | 0.125 W/m-K @Temperature 204 °C |
0.864 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Duratherm LT Paraffinic Heat Transfer Fluid Duratherm LT - heat transfer fluid engineered for applications requiring process temperatures ranging from -30°F to 600°F. Ideal for batch processing requiring heating and cooling cycles. Eliminat.. |