Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.110 W/m-K @Temperature 540 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are f.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 425 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 797 °F |
|
Pyrotek M-18 Compressible/Insulating Boards ApplicationsTrough, ladle and launder linings High temperature gaskets Mill board substitute AdvantagesWater moldable Excellent thermal shock resistance High compressibility Excellent resistance to .. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 630 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1170 °F |
|
Pyrotek PTB 2200 Structural Board ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 535 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 995 °F |
|
Pyrotek M-13 Compressible/Insulating Boards ApplicationsHigh temperature gaskets Non-conductive insulation Lid gaskets AdvantagesDurable Resistant to chemical attack Excellent mechanical strength Low air permeability Information provided by P.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 800 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 800 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 200 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group ISOPERLOR 550P Perlite Insulating Brick & Block ISOPERLOR perlite insulating bricks & blocks have the following characteristics: Max. service temperature 900°C (1652°F)Back-up insulation onlyExcellent insulating propertiesVery lightweight a.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 200 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group Moler HIPOROS Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 400 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 752 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-25/1700 Alumina Insulation AL-25/1700 is a rigid medium duty grade of alumina fiber board. Not as strong as SALI but capable of delivering years of service.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 600 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Zircar Ceramics ECO-1200A Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems. Information provid.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 600 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Zircar Ceramics ECO-1200B Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-1200 is part of hundreds of different thermal process systems. Information provid.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 800 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C177-76 |
Zircar Ceramics Uniform A1 Alumina-Silica Insulation ZIRCAR Alumina-Silica Insulation Type "UNIFORM A" is a family of refractory ceramic fiber based insulations with exceptional machineability and strength. They are made of specially prepared alumi.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 204 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Zircar Refractory Composites RSBD-HD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-HD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 649 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Zircar Refractory Composites RSBD-LD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-LD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 800 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 800 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 800 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 538 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1000 °F |
8 pcf blanket (Parallel to thickness) |
Zircar Ceramics ASB-2300 Alumina-Silica Blanket Useful to temperatures of 1260°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 316 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 601 °F |
|
BNZ Materials Marinite® I&M High Temperature Structural Insulation Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 800 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 600 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C177-76 |
Zircar Ceramics ASH Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its.. |
|||
Thermal Conductivity | 0.110 W/m-K @Temperature 600 °C |
0.763 BTU-in/hr-ft²-°F @Temperature 1110 °F |
parallel to thickness |
Zircar Ceramics ASQ Castertip 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform.. |