Thermal Properties Metric English Comments
Thermal Conductivity 0.0600 W/m-K

@Temperature 93.0 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 199 °F
Pyrotek I-14 Insulating Board
Pyrotek's I-14 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-14 also contains no RDF's.A..
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab
SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity..
Thermal Conductivity 0.0600 W/m-K

@Temperature 250 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 482 °F
parallel to thickness; ASTM C177-76
Zircar Ceramics ZAL-15AA Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C177
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE
ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped ..
Thermal Conductivity 0.0600 W/m-K

@Temperature 500 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 932 °F
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper
ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct..
Thermal Conductivity 0.0600 W/m-K

@Temperature 200 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C182
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation
Information provided by BNZ Materials Inc.
Thermal Conductivity 0.0600 W/m-K

@Temperature 250 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 482 °F
parallel to thickness; ASTM C177-76
Zircar Ceramics ZAL-15 Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.0600 W/m-K

@Temperature 500 °C
0.416 BTU-in/hr-ft²-°F

@Temperature 932 °F
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper
ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c..