Polymer Property : Thermal Conductivity = 1.45 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.25 - 1.45 W/m-K

@Temperature 100 °C
8.68 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 90 PF Moldable Refractory Material
Description: Curas 90 PF ramming mix with outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). The product is supplied in two components: a dry powder and a liquid. Curas 90 PF i..
Thermal Conductivity 1.25 - 1.45 W/m-K

@Temperature 100 °C
8.68 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 90 PF REPAIR Moldable Refractory Material
Description: Curas 90 PF Repair ramming mix is especially developed for repairing purposes of Curas 90 PF linings. The product is supplied in two components: a dry powder and a liquid. Detailed inst..
Thermal Conductivity 1.25 - 1.45 W/m-K

@Temperature 100 °C
8.68 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURAS 90 PFM Moldable Refractory Material
Description: Curas 90 PFM ramming mix has outstanding abrasion properties, (erosion loss acc. ASTM C704: 2-4 cm3). In addition, it has a good resistance against thermal shock and corrosive gasses. T..
Thermal Conductivity 1.35 - 1.45 W/m-K

@Temperature 100 °C
9.37 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 170 Dense Refractory Castable
Description: A general purpose castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks: These v..
Thermal Conductivity 1.35 - 1.45 W/m-K

@Temperature 100 °C
9.37 - 10.1 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 170 GM Dense Refractory Castable
Description: A general purpose gunning castable with a wide range of applications for high temperatures. The low Fe2O3 content makes this castable suitable for use under reducing conditions.Remarks:..
Thermal Conductivity 1.25 - 1.45 W/m-K

@Temperature 600 °C
8.68 - 10.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 180 T SP GM Dense Refractory Castable
Description: Curon 180 T SP GM is a gunning castable based on tabular alumina for application at very high temperatures.Remarks: These values apply to cast products.Information provided by Gouda Vuu..
Thermal Conductivity 1.35 - 1.45 W/m-K

@Temperature 600 °C
9.37 - 10.1 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast VIBRON 160 H GS (R) Dense Vibrating Refractory Castable
Description: Vibron 160 H GS (R) is a pumpable low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock-, corrosion- and abrasion resista..
Thermal Conductivity 1.25 - 1.45 W/m-K

@Temperature 1000 °C
8.68 - 10.1 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable
Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t..