Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.410 - 0.510 W/m-K @Temperature 600 °C |
2.85 - 3.54 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 145 Refractory Insulating Castable Description: Golite 145 can be used in direct contact with the furnace conditions and combines a high strength with a good thermal insulation.Remarks: These values apply to cast products. Also avail.. |
|||
Thermal Conductivity | 0.410 - 0.510 W/m-K @Temperature 600 °C |
2.85 - 3.54 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 155 Refractory Insulating Castable Description: Due to it's high strength at high temperatures, this material can be applied in direct contact with the firing process.Remarks: These values apply to cast products. Also available i.. |