Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 5.00 W/m-K @Temperature 100 °C |
34.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 98 Dense Refractory Brick Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette.. |
|||
Thermal Conductivity | 5.00 - 7.00 W/m-K @Temperature 1300 °C |
34.7 - 48.6 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURAS SiC 70 D GM Moldable Refractory Material Description: This gunning material is supplied as a dry powder. Curas SiC 70 D GM has a phosphate bond and is specially developed as a protection layer on boiler tubes.Remarks: The stated chemical c.. |
|||
Thermal Conductivity | 5.00 - 7.00 W/m-K @Temperature 100 °C |
34.7 - 48.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURAS SiC 90 D Moldable Refractory Material Description: This material is supplied as a dry powder. It has to be mixed with clean water to the necessary consistency. Curas SiC 90 has a phosphate bond and especially meant for protection of bo.. |
|||
Thermal Conductivity | 5.00 W/m-K @Temperature 100 °C |
34.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 99 Dense Refractory Brick Description: This high purity alumina based brick finds wide application in chemical reactors. The low percentages of SiO2 and Fe2O3 makes this brick very resistant in reducing conditions.Remarks: T.. |
|||
Thermal Conductivity | 5.00 - 7.00 W/m-K @Temperature 1300 °C |
34.7 - 48.6 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURAS SiC 70 D Moldable Refractory Material Description: This material is supplied as a dry powder and has to be mixed with clean potable water to the necessary consistency. Curas SiC 70D has a phosphate bond and is specially developed for b.. |
|||
Thermal Conductivity | 5.00 - 7.00 W/m-K @Temperature 100 °C |
34.7 - 48.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast VIBRON 160 K 50 Dense Vibrating Refractory Castable Description: Vibron 160 K 50 is a low cement castable based on silicon carbide and characterized by a very good thermal conductivity, high abrasion resistance and a good oxidation resistance up to 1.. |
|||
Thermal Conductivity | 5.00 - 6.00 W/m-K @Temperature 1400 °C |
34.7 - 41.6 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 162 K Sp Dense Vibrating Refractory Silicon Carbide Castable Vibron 162 K Sp is a low cement castable based on silicon carbide. This castable is characterized by a very good thermal conductivity, a high abrasion resistance and high resistance against oxidatio.. |