Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 27.9 W/m-K @Temperature 100 °C |
194 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Thermal Conductivity | 27.9 W/m-K @Temperature 300 °C |
194 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
International Mold Steel Daido DRM2 Matrix High-Speed Steel This matrix type high speed tool steel is available for warm and cold forging tools where critical performance is required. DRM2 prolongs service life due to its higher hardness and toughness than t.. |
|||
Thermal Conductivity | 27.9 W/m-K @Temperature 760 °C |
194 BTU-in/hr-ft²-°F @Temperature 1400 °F |
|
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |
|||
Thermal Conductivity | 27.9 W/m-K @Temperature 300 °C |
194 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
International Mold Steel DHA-World Die Cast & Forging Steel DHA-World is a high hardenability and high tough general use hot work die steel.Information provided by International Mold Steel |