Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.7 W/m-K @Temperature 700 °C |
171 BTU-in/hr-ft²-°F @Temperature 1290 °F |
|
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C) Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas.. |
|||
Thermal Conductivity | 24.7 W/m-K @Temperature 300 °C |
171 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |
|||
Thermal Conductivity | 24.7 W/m-K @Temperature 500 °C |
171 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Thermal Conductivity | 24.7 W/m-K @Temperature 760 °C |
171 BTU-in/hr-ft²-°F @Temperature 1400 °F |
|
Haynes 617 Nickel Alloy Plate Haynes 617 alloy is a nickel-chromium-cobalt-molybdenum alloy with a good combination of metallurgical stability, strength, and oxidation resistance at high temperatures. The alloy is readily formed.. |