Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 3.2 mm thick sheet, GTAW weld HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 30% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 50% cold rolled and 5000 hours at 500°C, air cooled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, plate and bar HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 201LN Austenitic Stainless steel AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 304 Austenitic Stainless steel AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 304L Austenitic Stainless steel AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 305 Austenitic Stainless steel AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 316L Austenitic Stainless steel AK Steel 316L is an extra-low carbon version of AK Steel 316 that minimizes harmful carbide precipitation due to welding.Information provided by AK Steel |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 40% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, Annealed (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 60% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 40% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 0% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 40% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 60% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 20% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 20% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 500 °C |
149 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 0.71 mm thick sheet HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 10% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate, GTAW short arc weld 1.1 mm diameter filler wire HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 19.1 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 31.8 mm thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |
|||
Thermal Conductivity | 21.4 W/m-K @Temperature 600 °C |
149 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Haynes Hastelloy® G-30® alloy, 12.7 mm (1/2 in.) thick plate HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxidizin.. |