Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 177.4 W/m-K @Temperature 25.0 °C |
1231 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
Osprey Metals CE17 Al-Si Controlled Expansion Alloy Al-27%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |