Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 20.0 °C |
111 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 100 °C |
111 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 300 °C |
111 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Thermal Conductivity | 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |