Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 15.0 W/m-K @Temperature 204 °C |
104 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Latrobe MP35N® Alloy MP35N is a nickel-cobalt base alloy of the Multiphase alloy system that has a unique combination of properties - ultra high strength, toughness, ductility, and outstanding corrosion resistance. The .. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 300 °C |
104 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 300 °C |
104 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 100 °C |
104 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
AK Steel 13-4 SR® Ferritic Stainless Steel AK Steel 13-4 SR Stainless Steel is a ductile weldable ferritic with 13% Cr and 3.75% Al. The high aluminum content results in a base alloy with high electrical resistivity. It is intended for use w.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 23.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 23.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 23.0 °C |
104 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
condition H 900 |
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Thermal Conductivity | 15.0 W/m-K @Temperature 300 °C |
104 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |