Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.780 W/m-K @Temperature 550 °C |
5.41 BTU-in/hr-ft²-°F @Temperature 1020 °F |
|
Pyrotek Pyrocast AR PLUS Castable Refractory Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed... |
|||
Thermal Conductivity | 0.780 - 0.880 W/m-K @Temperature 1300 °C |
5.41 - 6.11 BTU-in/hr-ft²-°F @Temperature 2370 °F |
|
Gouda Vuurvast CURON 160 HF Dense Refractory Castable Description: This castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HF has an excellent thermal shock resistance. It is largely used in the .. |
|||
Thermal Conductivity | 0.780 - 0.880 W/m-K @Temperature 100 °C |
5.41 - 6.11 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Thermal Conductivity | 0.780 - 0.880 W/m-K @Temperature 100 °C |
5.41 - 6.11 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 13 SC Dense Refractory Castable Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho.. |
|||
Thermal Conductivity | 0.780 - 0.880 W/m-K @Temperature 100 °C |
5.41 - 6.11 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast CURON 14 S Dense Refractory Castable Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem.. |
|||
Thermal Conductivity | 0.780 W/m-K @Temperature 815 °C |
5.41 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Pyrotek Pyrocast TG Castable Refractory Pyrocast TG is a technical-grade silica based refractory developed for the non-ferrous industry including nickel, copper, zinc, and their alloys.ApplicationsCoreless induction furnace lining Channel.. |
|||
Thermal Conductivity | 0.780 - 0.880 W/m-K @Temperature 1500 °C |
5.41 - 6.11 BTU-in/hr-ft²-°F @Temperature 2730 °F |
|
Gouda Vuurvast GOLITE 180 Refractory Insulating Castable Description: Hollow alumina spheres are used as an aggregate for this castable. With very low percentages of Fe2O3 and SiO2, it is well resistant against reducing and corrosive kiln atmospheres.Rema.. |