Thermal Properties Metric English Comments
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 120 Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 has good thermal shock resistance.Remarks: These values apply to cast products. Also avai..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 120 HS Dense Refractory Castable
Description: This castable has a very good resistance against thermal shocks because of its low thermal expansion. In addition, it has a high strength. Used in incinerators and for tunnel kiln cars...
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 100 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 127 S Dense Refractory Castable
Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 600 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable
Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 600 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable
Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 100 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 160 HC Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 815 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Gouda Vuurvast CURON 100 Dense Refractory Castable
Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable
Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by ..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable
Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 1000 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast CURON 130 HRCC RAPID Dense Refractory Castable
Description: An extra coarse, low iron castable for use to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRCC RAPID has good thermal shock resistan..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 100 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 145 C Dense Refractory Castable
Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information ..
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 100 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast CURON 145 Dense Refractory Castable
Description: Because of the use of pure raw materials, Curon 145 has a low Fe2O3 content. Therefore this castable is widely used in reducing atmospheres.Remarks: These values apply to cast products...
Thermal Conductivity 0.550 W/m-K

@Temperature 200 °C
3.82 BTU-in/hr-ft²-°F

@Temperature 392 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul..
Thermal Conductivity 0.550 W/m-K

@Temperature 200 °C
3.82 BTU-in/hr-ft²-°F

@Temperature 392 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-56 MOLDABLE Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-56 Moldable is a high silica fiber reinforced ceramic composite material that is easily cut and formed into flat sheets in addition to a wide variety of simple and ..
Thermal Conductivity 0.550 W/m-K

@Temperature 200 °C
3.82 BTU-in/hr-ft²-°F

@Temperature 392 °F
parallel to thickness; ASTM C1113
Zircar Refractory Composites RSLE-57 Refractory Sheet
ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl..