Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.233 W/m-K @Temperature 260 °C |
1.61 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories GUN-100L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.233 W/m-K @Temperature 260 °C |
1.61 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories GUN-80L Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.233 W/m-K @Temperature 260 °C |
1.61 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories INCT-120S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.233 W/m-K @Temperature 1000 °C |
1.61 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Chosun Refractories INCT-80S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.233 - 0.4653 W/m-K @Temperature 540 °C |
1.61 - 3.224 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.233 - 0.291 W/m-K @Temperature 800 °C |
1.61 - 2.01 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Chosun Refractories MIX-2 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |