Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.200 W/m-K @Temperature 400 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek Insural® 85 MASTIC Insulating Mastic for Aluminum contact Applications Insural® 85 MASTIC is an asbestos-free, durable and insulating refractory composition designed for the fabrication of launders and jointing, bedding and patching of precast refractory shapes.Advant.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 400 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek Insural® GP MASTIC Insulating mastic for general-purpose refractory applications Insural® GP Mastic is an asbestos-free, durable and insulating refractory fiber composition designed for general-purpose patching and veneering applications that are not exposed to contact with mol.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 300 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 572 °F |
(DIN 51046)+ |
Pyrotek Pyrite B-3 Refractory Board Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 500 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 932 °F |
(DIN 51046)+ |
Pyrotek Pyrite B-3 Refractory Board Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 540 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 760 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1400 °F |
|
Pyrotek Pyrocast L-40 Insulating Refractory Pyrocast L-40 is a fiber free refractory moldable designed for use in contact with molten aluminum. L-40 has excellent workability for use as an insulating lining or patching material.Recommended C.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 100 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
Thermal Conductivity | 0.200 - 0.300 W/m-K @Temperature 100 °C |
1.39 - 2.08 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 125 R GM Refractory Insulating Castable Description: Golite 125 R GM has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products.Informati.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 816 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 600 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1110 °F |
BS 1902 Section 5.5 1991 |
Skamol Group Moler 10 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 600 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1110 °F |
BS 1902 Section 5.5 1991 |
Skamol Group Moler 5 Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 600 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1110 °F |
BS 1902 Section 5.5 1991 |
Skamol Group Moler BB-Filler Aggregate Insulation SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 600 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group Moler ROTOL Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 200 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group SKAMOCAST 112-80 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 400 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 752 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics SALI Alumina Insulation SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 1010 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1850 °F |
|
Zircar Refractory Composites RSBD-LD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-LD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 800 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C177 |
Zircar Refractory Composites RS-C ALUMINA-SILICA MOLDABLE ZIRCAR Alumina-Silica Insulating Blanket Type RS-C Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped .. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 800 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 816 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Tritex TRI-F Blanket Insulation TRI-F is a unique thermal and acoustic insulation that combines three high temperature fibers in a patented process. The result is a blanket with a service life to 1500°F. By blending fibers of var.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 816 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-23A Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 816 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-24 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 400 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 400 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials BNZP-26A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 260 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials PA 20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 1100 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 2010 °F |
ASTM C177-76 |
Zircar Ceramics ASH Alumina-Silica Insulation ZIRCAR Ceramics Alumina-Silica Insulation Type ASH is one of the first alumina-silica products produced by ZIRCAR. Made of bulk fiber and inorganic alumina binders Type ASH is uniform throughout its.. |
|||
Thermal Conductivity | 0.200 W/m-K @Temperature 800 °C |
1.39 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |