Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.190 W/m-K @Temperature 1400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 50.0 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1.. |
|||
Thermal Conductivity | 0.190 - 0.290 W/m-K @Temperature 600 °C |
1.32 - 2.01 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GI 23 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.190 - 0.290 W/m-K @Temperature 100 °C |
1.32 - 2.01 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |
|||
Thermal Conductivity | 0.190 - 0.290 W/m-K @Temperature 600 °C |
1.32 - 2.01 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 600 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group Moler LR-1750 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 600 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (475) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (700) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (700) Panel Design SKAMOLEX panel designs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatil.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group SKAMOLEX V-1100 (800) Customized Shape SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 600 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group V-1100 475 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 600 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group V-LITE 475 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1075 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1967 °F |
Parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1075 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1967 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1100 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 2010 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 800 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 538 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Zircar Ceramics APA-3 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 400 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials BNZP-23 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 600 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials BNZP-23L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 1075 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 1967 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.190 W/m-K @Temperature 50.0 °C |
1.32 BTU-in/hr-ft²-°F @Temperature 122 °F |
|
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |