Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.170 W/m-K @Temperature 815 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Pyrotek AL-THERM 2100H Vacuum formed refractories for use with modular hot top systems Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are f.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group Moler BB-BLOCK Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 400 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group Moler LR-1750 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group V-1100 410 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTMÂ C-182 |
Skamol Group Moler SM-65 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 980 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1800 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 800 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Ceramics AXL Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 980 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1800 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics MB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 800 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1470 °F |
ASTM C177-76 |
Zircar Ceramics Uniform A2 Alumina-Silica Insulation ZIRCAR Alumina-Silica Insulation Type "UNIFORM A" is a family of refractory ceramic fiber based insulations with exceptional machineability and strength. They are made of specially prepared alumi.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 649 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Zircar Refractory Composites RSBD-HD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-HD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 1100 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 1100 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 2010 °F |
parallel to thickness |
Zircar Refractory Composites RS-3000 ALUMINA FELT ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 538 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-20 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 537 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 999 °F |
|
3M 615+ Fire Barrier Duct Wrap 3M Fire Barrier Duct Wrap 615+ is a flexible fire-resistant wrap consisting of an inorganic fiber blanket encapsulated with a scrim-reinforced foil. The product is 1-1/2 in. thick, 6pcf density. It .. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 7962MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 9172MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 467MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Thickness 0.0508 mm |
1.18 BTU-in/hr-ft²-°F @Thickness 0.00200 in |
|
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 600 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
3M Nextel™ AF-14 Industrial Woven Fabric 312 Information provided by 3M |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 200 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
DuPont Performance Polymers Kalrez® 1050LF FFKM Perfluoroelastomer A general-purpose compound for O-rings, seals, and other parts used in chemical process industries. It has good hot water/steam, excellent amine resistance, and enhanced compression set properties... |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 200 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen.. |
|||
Thermal Conductivity | 0.170 W/m-K @Temperature 200 °C |
1.18 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer
(discontinued **) A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application.. |