Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.104 W/m-K @Temperature 204 °C |
0.720 BTU-in/hr-ft²-°F @Temperature 400 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |
|||
Thermal Conductivity | 0.104 W/m-K @Temperature 538 °C |
0.722 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek AFB-2300 HT Structural Board AFB-2300 HT is a ceramic fiber board which features a unique alumina-based binder. This white board is heat-treated to eliminate all possible out-gassing and withstands temperatures up to 1260°C.H.. |