Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0800 W/m-K @Temperature 260 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Pyrotek M-18 Compressible/Insulating Boards ApplicationsTrough, ladle and launder linings High temperature gaskets Mill board substitute AdvantagesWater moldable Excellent thermal shock resistance High compressibility Excellent resistance to .. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 315 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 599 °F |
|
Pyrotek M-13 Compressible/Insulating Boards ApplicationsHigh temperature gaskets Non-conductive insulation Lid gaskets AdvantagesDurable Resistant to chemical attack Excellent mechanical strength Low air permeability Information provided by P.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 204 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Pyrotek Pyrocast L-30 Moldable Refractory Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommen.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-182 |
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Ceramics AXHTM Alumina-Silica Insulation ZIRCAR Alumina Silica Insulation Type AXL and Type AXHTM are inorganically bound insulation boards typified by their rigid outer surfaces and unbound interiors. They offer low thermal conductivity a.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 525 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 977 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 800 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 500 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Zircar Refractory Composites ASPA-880 Alumina-Silica Fiber Paper ASPA-880 is a high temperature, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. It is made from shorter and smaller diameter fibers with a higher .. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 500 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 932 °F |
parallel to thickness |
Zircar Refractory Composites RS-3000 ALUMINA FELT ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTM C182 |
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 400 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 525 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 977 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 800 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Thermal Conductivity | 0.0800 W/m-K @Temperature 870 °C |
0.555 BTU-in/hr-ft²-°F @Temperature 1600 °F |
|
Pyrotek M-12 Compressible/Insulating Boards ApplicationsHigh temperature gaskets Furnace covers Trough lining AdvantagesLow density Good insulating ability Information provided by Pyrotek. |