Polymer Property : Maximum Service Temperature, Air = 716 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 380 °C
716 °F
Continuous
Aremco Aremco-Seal™ FO-380 High Temperature Specialty Coatings Silicone, Ceramic Filled  (discontinued **)
Hi-temp, waterborne silicone adhesive and sealant used to pot fiber optic strands into stainless steel ferrules. Typically used in applications to 716 °F (380 °C). Low viscosity, easy to use, offe..
Maximum Service Temperature, Air 380 °C
716 °F
Synergy Polymers Ultra Purge HT
Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean..