Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 287 °C | 549 °F | Deflection Temperature, Load not specified; ASTM D648 |
Quantum Composites AMC™ 8590 BK 53% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8590 BK is a vinyl ester, chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant,.. |
|||
Maximum Service Temperature, Air | 287 °C | 549 °F | Deflection Temperature, Load not specified; ASTM D648 |
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat .. |
|||
Maximum Service Temperature, Air | 287 °C | 549 °F | Deflection Temperature, Load not specified; ASTM D648 |
Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC AMC™ 8593 NT is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high he.. |
|||
Maximum Service Temperature, Air | 287 °C | 549 °F | Deflection Temperature, Load not specified; ASTM D648 |
Quantum Composites AMC™ 8595 55% Carbon Fiber Reinforced Vinyl Ester SMC AMC™ 8595 is a vinyl ester engineered structural composite molding compound with continuous, unidirectional carbon fibers. It is designed for compression molding of components requiring high struc.. |