Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Precision Polymer Engineering Perlast® G50S FFKM White Perfluoroelastomer Perlast® G50S FFKM is a White Perfluoroelastomer 50-55 °IRHD. It has excellent chemical resistance, steam resistance and mechanical properties. Suitable for use in all food applications, and extr.. |
|||
Maximum Service Temperature, Air | >= 260 °C | >= 500 °F | Shear Adhesive Failure (polyester failure) |
Dielectric Polymers NT-5513 High Tack Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
Maximum Service Temperature, Air | >= 260 °C | >= 500 °F | Shear Adhesive Failure (polyester failure) - silicone side |
Dielectric Polymers NT-1020 Silicone/Acrylic Double Coated Tape
(discontinued **) Crosslinked silicone and acrylic adhesive with 2 mil polyester film release liner backing on the silicone side and moisture stable PE coated kraft (60#) on the acrylic side.Features: Chemical resist.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous |
Dielectric Polymers TRANS-SIL® NT-1001 Silicone Transfer Adhesive
(discontinued **) Crosslinked silicone adhesive with 2 polyester film release liners.Features: Resistant to extreme temperaturesHigh bond strengthChemical resistantApplications: High performance bonding and other app.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | short term |
Lehmann & Voss LUVOCOM® 1105-8174 PEEK, with PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Maximum Service Temperature, Air | 260 °C @Pressure 8.27 MPa |
500 °F @Pressure 1200 psi |
Continuous |
Garlock GYLON® 3540 Microcellular PTFE Gasketing Microcellular PTFE.Highly compressible PTFE seals under low bolt load- suitable for many non-metallic flangesCompressible material conforms to surface irregularities, especially on warped, pitted or.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous |
Momentive Performance Materials RTV106 One Component Acetoxy Adhesive Sealant, Red RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Guarniflon PFA Perfluoroalkoxy Polymer Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain Chemlam® SGC6-06 Copper Adhesive Tape Description: Chemlam® Copper SGC6 is fiberglass fabric impregnated with PTFE (polytetrafluoroethylene) dispersion, laminated to PTFE film and coated with high-temperature, pressure-sensitive sili.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | UL-746 B |
Saint-Gobain Norton® F910 FDA Compliant Skived PTFE Sheet Description: PTFE = polytetrafluoroethyleneApplications include: FDA Compliant; Common in Electronics/ElectricalInformation provided by Saint Gobain Performance Products. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® 2255-3 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain CHR® K290ESD Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Saint-Gobain Chemfab® SlipGrip™ 3 PTFE/Silicone Coated Fiberglass Fabric Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. .. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Master Bond EP46HT-2Med Two Component Heat Resistant Biocompatible Epoxy System Master Bond Polymer System EP46HT-2MED is a two component medical grade epoxy system for high performance structural bonding and casting suitable for applications where resistance to temperatures fr.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Short Term (3h) |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Extended |
Hexcel® HexWeb® HRH-327 - 3/8 - 5.5 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Trelleborg Emerson & Cuming Stycast® 5954 Two-Component Silicone High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous use |
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder 30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Short term |
3M 9499 Splicing Tape 3M™ Splicing Tapes utilize an acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
BASF Paliotol™ Yellow K 0961 HD Color Additive Chemical Structure: Chinophthalone Yellow Application: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, CA/CAB, and UPRecommendations for food applications: BgVV, FDA, Franc.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Short Term |
3M VHB™ F9469PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous Service |
Solvay Specialty Polymers Algoflon® F3140 X PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |
|||
Maximum Service Temperature, Air | >= 260 °C | >= 500 °F | Shear Adhesive Failure (polyester failure) |
Dielectric Polymers NT-582 Plating Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Fine line definitionClean tape removalGood conformabilityChemical resistantApplications: For PCB masking during the solder strip b.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | short term |
Lehmann & Voss LUVOCOM® 1105-8135/OR PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous Service |
Solvay Specialty Polymers Algoflon® F6 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
DuPont Performance Polymers Kalrez® 6221 FFKM Perfluoroelastomer Kalrez® parts made from compounds 6221 provide superior chemical resistance and low contamination from extractables in pharmaceutical and food handling applications where FDA compliance is required.. |
|||
Maximum Service Temperature, Air | 260 °C | 500 °F | |
Master Bond Supreme 46HT-2ND2 Two Component, Non-Drip, Toughened, Epoxy Adhesive Master Bond Polymer Supreme 46HT-2ND2 is a two component, non-drip, epoxy adhesive featuring an attractive balance of superior shear and peel strengths for high performance structural bonding suitab.. |