Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 246 °C | 475 °F | Long Term |
Quadrant EPP Semitron® 480 ESd PEEK, static dissipative, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsThis PEEK based static dissipative material provides a dissipative range of 10E+6 - 10E+9 ohms/sq. Semitron® ESd 480 is very dimensionally sta.. |
|||
Maximum Service Temperature, Air | 246 °C | 475 °F | Long Term |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |