Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 221 °C | 430 °F | Long Term |
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet) |
|||
Maximum Service Temperature, Air | 221 °C | 430 °F | |
Aremco Aremco-Bond™ 2340 High Temperature Epoxide Potting Compound High Temperature, Low Viscosity, Low Expansion, High Glass Transition Temperature & Chemical Resistance |