Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 204 °C | 400 °F | |
ND Industries 460 Instant High Pressure Pipe Sealant High temperature, high strength general purpose stainless steel and other inert metals. For metal fittings |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Constant |
Plasma Coatings 15000 Surface Material Information provided by Plasma Coatings |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Dielectric Polymers NT-511 High Temperature Tape
(discontinued **) Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Garlock 502 Silicone Sheet Rubber Style #502 will be used in sealing applications that require resistance to extreme temperatures, high ozone concentrations, and high ultraviolet content.Information provided by Garlock Rubber Techno.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | continuous |
Lucas-Milhaupt Silvaloy® A35 Brazing Alloy Silvaloy A35 is a good general purpose alloy often used when cadmium must be avoided such as in the dairy and food industries. It is used for brazing in the electrical industry and for brazing brass.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | continuous |
Lucas-Milhaupt Silvaloy® 50 Brazing Alloy Silvaloy is one of the lower melting brazing alloys composed of silver, copper, zinc and cadmium. It is suitable for use on most metals except aluminum and magnesium. It is used for joining steel, s.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond FL901S Silver Filled, Electrically Conductive Adhesive Film Master Bond FL901S Polymer System is a high performance silver filled unsupported epoxy resin based adhesive film which offers outstanding performance characteristics and does not require refrigerat.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Mastersil 701 One Component, Room Temperature Curing Silicone Elastomer Master Bond Master Sil 701 is a ready-to-use, one component, high performance silicone elastomer compound for bonding, and sealing protective coatings and formed-in-place gaskets. It cures at ambien.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond MasterSil 705C Non-Corrosive Silicone with Carbon Filler Description: Master Bond MasterSil 705C is an electrically conductive, one component, non-corrosive, carbon filled silicone for bonding, sealing and coating. This black colored paste like system cur.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Supreme 10AOHT-LO High Shear and Peel Strength Epoxy Description: Master Bond Supreme 10AOHT-LO has a combination of properties consisting of excellent thermal conductivity, superior electrical insulation, great adhesion to a wide variety of substrate.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Master Bond Supreme 10HTF Fast Curing Toughened One Component Epoxy Adhesive Master Bond Polymer System Supreme 10HTF is a one part, no-mix system featuring a unique combination of properties including high shear and peel strength, exceptionally wide service temperature rang.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Loctite® PST® 580 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Loctite® PST® 592 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
CIP Composites 300 Series Laminated Polymer Bearing Material The 300 series consists of Nomex® fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated p.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Cotronics Bond-It™ 7040 Epoxy, Room Temperature Cure Forms high strength bonds to difficult metals, plastics, glass, ceramics, composites, etc. Cures at room temperature with high temperature strength and good electrical and thermal shock resistance... |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Abatron L060421-1 Heat-Resistant (-75~400°F) Non-Flammable Silicone Rubber L060421-1 is a heat-resistant and non-flammable silicone rubber recommended as a potting compound for exceptional protection against thermal shock, vibration, moisture, ozone, dust, chemicals, and o.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon 920-10R##-P2 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon CP-499CA Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon LW202Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon LW301C##FR-P1 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 30 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon Thermabond® R36211A008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation II Thermabond® NP electrically insulating electronic adhesive. Bonds without primerDesign/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: St.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Continuous |
Arlon 51393R032 0.032" (0.813 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: Temperature and time dependentThis data represents typical values for the production material. The data shoul.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | |
Arlon R35798R013 0.013" (0.330 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 Fiberglass Side 2: Uncured Silicone RubberThis data represents typic.. |
|||
Maximum Service Temperature, Air | 204 °C | 400 °F | Constant |
Plasma Coatings 26000 Surface Material Information provided by Plasma Coatings |