Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1430 °C | 2600 °F | Short term |
Mid-Mountain Materials HYTEX® 2200 Ceramic Fiber Industrial Textile HYTEX® 2200 Ceramic Fiber Industrial Textiles are exceptionally effective high temperature textile products capable of withstanding continuous temperatures up to 2200ºF (1205ºC). Manufactur.. |
|||
Maximum Service Temperature, Air | 1430 °C | 2600 °F | |
Cotronics Resbond™ 901 High Temperature Ceramic Adhesive, Fiber Base Single component system with a paint consistency. |
|||
Maximum Service Temperature, Air | 1430 °C | 2600 °F | |
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required. |
|||
Maximum Service Temperature, Air | 1430 °C | 2600 °F | Continuous |
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Maximum Service Temperature, Air | 1430 °C | 2600 °F | Continuous |
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |