Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 127 °C | 260 °F | Long Term |
Quadrant EPP Nylatron® MC® 901 Blue, Heat Stabilized, Type 6 (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic ProductsBroadest size range availabilityGood mechanical and electrical propertiesIdeal balance of strength and toughnessCast as finished parts and near .. |
|||
Maximum Service Temperature, Air | 127 - 150 °C | 260 - 302 °F | Average value: 140 °C Grade Count:34 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Maximum Service Temperature, Air | 127 °C | 260 °F | continuous |
Ensinger Hydel® PC-7 Polycarbonate (PC) A polycarbonate based material with a proprietary carbon filler component. The highly dispersed filler imparts outstanding electrical consistency to minimize any hot spots. The material has good r.. |
|||
Maximum Service Temperature, Air | 127 °C | 260 °F | Long Term; ASTM UL746B |
Ensinger Tecast Vekton™ 6XAU High Heat Cast Nylon 6 (PA6) VEKTON® 6XAU is a high heat weather resistant cast nylon 6 with superior fatigue-resistant and bearing properties.General Vekton® Cast Nylon Information: VEKTON cast nylon, available in a variety .. |
|||
Maximum Service Temperature, Air | 127 °C | 260 °F | |
Quantum Polycarbonate 20% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |