Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast CURON 130 Dense Refractory Castable Description: Curon 130 is a castable with a good workability and a high strength. Therefore this castable can be characterized as a reliable refractory construction material.Remarks: These values ap.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast GI 23 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast B Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Gouda Vuurvast CURON 13 SC Dense Refractory Castable Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics HFI Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics MH 30 Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics REFCAST NORMAL Dense Castables Description: We offer a range of Dense Castables that are conventional castable and extensively used in boiler work, general furnace and burner blocks. Made as per international standards, our range.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics Sharada LTM 0.9 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Sharadaa Ceramics Sharada LTM 1.0 Insulating Castable Low Density/ High Strength Insulating Castable-Low Thermal Mass LiningInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ 350 Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ CG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ SG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | Deformation temp |
SPHERE ONE EXTENDOSPHERESâ„¢ TG Hollow Spheres EXTENDOSPHERESâ„¢ hollow spheres are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, t.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Zircar Refractory Composites RS-MS ALUMINA MOLDABLE SLEEVING ZIRCAR Refractory Sheet Type RS-MS Moldable Sleeving is a moist woven alumina composite sleeving. It is supplied in a wet form ready for the fabrication of custom shapes. It can be cut to size with .. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Zircar Refractory Composites RS-Tape Refractory Sheet Refractory Sheet RS-Tape is ceramic fiber reinforced alumina composite. It offers the strength, durability, flexibility and versatility required by many high temperature applications up to 1300°C(2.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | limited |
Chosun Refractories BCT-130 Acid-proof Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | limited |
Chosun Refractories CT-130 Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Maximum Service Temperature, Air | >= 1300 °C | >= 2370 °F | |
China-Yixing Longly Refractories 75 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | limited |
Chosun Refractories PTC-130S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Maximum Service Temperature, Air | 1300 °C | 2370 °F | |
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
Maximum Service Temperature, Air | 1300 - 1600 °C | 2370 - 2910 °F | |
CeramTec SL200B Silicon Nitride SL200B ceramic material was designed especially for use in the field of welding technology. SL200B is a 100 bar gas-pressure sintered silicon nitride (Si3N4) with impressive properties. It boasts de.. |