Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek J-1 Ropes Available in braided or twisted form. Excellent tensile strength and abrasion resistance. Low thermal conductivity.AdvantagesExcellent Abrasion Resistance Fair Compression and Recall Information p.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Continuous |
Pyrotek M-18 Compressible/Insulating Boards ApplicationsTrough, ladle and launder linings High temperature gaskets Mill board substitute AdvantagesWater moldable Excellent thermal shock resistance High compressibility Excellent resistance to .. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Continuous |
Pyrotek M-2 Fiber Seal Pre-cut Gasket A light-brown ceramic fiber material. Excellent trough gasket material.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek Pyroboard™ S1300 Roller Pyroboard™ S1300 was developed specifically for use in hotter zones of an annealing furnace.Information provided by Pyrotek. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Pyrotek Vacuum Formed Shapes for Continuous Sheet Casting Vacuum formed shapes are manufactured from high purity alumina silica fibers in one-piece design that eliminates metal leakage. No pre-heating required. Reusable, with proper treatment, for multip.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Continuous Use Limit |
ICHS Fiberfax® Alumina-Silica Ceramic Fibers Fiberfrax® ceramic fibers are made from high-purity alumina-silica materials. ICHS uses Fiberfrax® ceramic fiber to manufacture vacuum-formed products in:High-Temperature DuctworkCombustion C.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Intermittent |
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Use Limit |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Use Limit |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® T22 Tamping Mix Description: THERMOSEAL® T22 FIBERPAK® TAMPING MIX is a wet taping mix made up of bulk refractory fibers and a high temperature binder system. T22 FIBERPAK® TAMPING MIX is particularly good.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Sharadaa Ceramics And Bulk Fiber Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Ceramics Z-MAG/2300 Soluble Fiber Insulation ZIRCAR NON-RCF Insulation Type Z-MAG/2300 is a rigid combination of soluble NON-RCF silica magnesia glass fibers and inorganic binder. It is suitable for use as a substitute for insulation containin.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites RSBD-HD ALUMINA-SILICA INSULATION ZRCI Alumina-Silica Insulation Type RSBD-HD Board is a ceramic fiber insulation suitable for use to 1260°C (2300°C). It is a strong, rigid refractory structure of high temperature ceramic fibers a.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites RSPA-SOL3 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Ceramics AS-1260 Alumina-Silica Textile Multiple forms of ceramic fiber textiles made of reinforced yarn. Amazingly strong, they are useful as gasketing, insulation and fire protection to temperatures of 1260°C (2300°F).Information pro.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Ceramics ASB-2300 Alumina-Silica Blanket Useful to temperatures of 1260°C this mechanically needled ceramic fiber blanket is available in a variety of thickness' and densities. Information provided by Zircar Ceramics. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites ASPA-2 Alumina-Silica Fiber Paper ASPA-2 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Refractory Composites RS-201 Refractory Sheet ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Cotronics Resbond™ 907 High Temperature Ceramic Adhesive, Industrial Strength |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
BNZ Materials Blazecrete 2300 ARG Dense Castable Blazecrete 2300 ARG is an alumina-silica castable with high strength and abrasion resistance. For service to 2300°F (1260°C). May be gunned or slap-troweled over Blaz 2000G to obtain a high streng.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Recommended Operating Temperature |
Unifrax Fiberfrax® Duraset® Flet Fiberfrax® Lo-Con™ felt and Duraset® flet are unique product forms in the Unifrax Corporation's extensive ceramic fiber product family. Felt products extend the performance of Fiberfrax papers i.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | |
Zircar Ceramics ECO-27B Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer.. |
|||
Maximum Service Temperature, Air | 1260 °C | 2300 °F | Continuous |
Pyrotek M-3 Fiber Seal Pre-cut Gasket A resin-coated felt. Repels water.Information provided by Pyrotek. |