Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | >= 107 °C | >= 225 °F | |
Parker Chomerics CHO-FLEX 601 Conductive Coating CHO-FLEX™ 601 coating is specifically designed for EMI shielding of copper/Kapton flexible circuit laminates and for printing circuits on Kapton film. Upon cure, this coating exhibits excellent adh.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Parker Chomerics CHO-FLEX 602 Conductive Coating CHO-FLEX™ 602 is a two-component silver-filled polyurethane coating designed for room temperature or oven cure. CHOFLEX™
602 coating can be sprayed on large panels, cured at room temperature and .. |
|||
Maximum Service Temperature, Air | >= 107 °C | >= 225 °F | |
Henkel Hysol EA 9360 Paste Adhesive System Structural adhesive, exhibits excellent peel strength, tensile lap shear strength.Applications: Structural Repair Composite Bonding Liquid Shim |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Saint-Gobain CHR® 2300-10R UHMW Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: UHMW polyolefin film tape provides anti-sticking and abrasion resistance properties for application temperatures ranging from -100°F to 225°F (-73°C to +107°C). Applications.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Loctite® 312 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
Loctite® 410 Toughened Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Continuous |
DuPont™ Tedlar® SP TTR10AH9 Transparent Polyvinyl Fluoride Film Transparent, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistanc.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Continuous |
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film Transparent, Medium Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resista.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Continuous |
DuPont™ Tedlar® TTR10BG3 Transparent Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
ConocoPhillips EP Conolith® Grease NLGI NO. 00 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
ConocoPhillips EP Conolith® Grease NLGI NO. 000 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 420 Lead Foil Tape Linered plasting tapeInformation provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 472 Vinyl Tape 3M™ Vinyl Tape 472 is comprised of a heavy duty backing with a black pigmented rubber adhesive. The thick vinyl backing makes it ideal for applications requiring both abrasion resistance and the in.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 6035PC 12056 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 6035PC 12062 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ6008 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M Scotchcal™ ElectroCut™ 406 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | for 50% loss of tensile strength after 20000hr |
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned) Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent |
3M SJ5201 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 3325 Copper Foil Tape EMI/RFI shielding. UL 510 Recognized.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 5423 Polyethylene Tape 3M™ Polyethylene Tape 5422 has a rubber adhesive which provides an excellent abrasion resistant surface.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 5425 UHMW Polyethylene Tape 3M™ UHMW Polyethylene Tape 5425 is a film coated with a special acrylic adhesive that is resistant to many solvents.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 5430 Squeak Reduction Tape 3M™ Squeak Reduction Tapes are a film tape for the automotive industry to help control squeaks and rattles due to vibration or wear of metal and plastic materials.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M 6035PC 12049 Polyurethane Foam Tape (20 lb./ft3 (320 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ6232 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Intermittent Exposure |
3M Bumpon™ SJ5808 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | |
3M Scotchcal™ ElectroCut™ 405 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | ASTM D1329 |
Seals Eastern 7045 Ethylene-Propylene Rubber General service EPDM.Information provided by Seals Eastern, Inc. |
|||
Maximum Service Temperature, Air | 107 °C | 225 °F | Shear Adhesive Failure (cohesive failure) |
Dielectric Polymers NT-988 High Tack Laminating Adhesive
(discontinued **) Acrylic copolymer adhesive with silicone treated release paper liner.Features: Excellent adhesion to low surface energy substratesCompatible with most printing inksApplications: Mounting a wide vari.. |