Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 48.9 °C | 120 °F | wet |
ITW Devcon Flexane® Rubber Repair / Castable Urethane Belt Repair Kit, Black Information provided by ITW Devcon |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Long Term |
3M 4466W Double Coated Polyethylene Foam Tape 3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Long Term |
3M 9456 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM002 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM024 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM03R2 Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM05E Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM062 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM065 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM110 Indoor UL Recognized Brushed Silver Polyester Label Products 3M™ Indoor UL Recognized Brushed Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utili.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM127 Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FP021 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FP022101 White Polypropylene Label Product 3M™ White Polypropylene Label Products FP022101, FP022102, FP022108, FP026002, FP02600N and FP026009 are matte white opaque materials that offer excellent durability and moisture resistance. These .. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FP022202 White Polypropylene Label Products 3M™ White Polypropylene Label Products FP022202 is a white opaque material that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1480, which is a high.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FP089 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FS023 Clear Polystyrene Label Products 3M™ Clear Polystyrene Label Products are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, which is a high c.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FV091 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FV517 Semi-Rigid Vinyl Label Product 3M™ Semi-Rigid Vinyl Label Products are semi-rigid white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1410, which is a general purpose.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FVT40 Tire Label Product 3M™ Tire Label Products utilize a flexible and conformable white vinyl labelstock that offers durability, moisture resistance, and dimensional stability. 3M™ Adhesive G1120, a rubber-based aggress.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M 7025 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M 8087 Construction Seaming Tape 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FL01000N Lexan Label Product 3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high .. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM068 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Service |
3M FS442 Matte Clear Polystyrene Label Products 3M™ Matte Clear Polystyrene Label Products FS442 is a hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, whic.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FS501 White Polystyrene Label Products 3M™ White Polystyrene Label Products FS501, FS502 and FS532 are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive R.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FV032R Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M OFM0302 Outdoor UL Recognized White Polyester Label Product 3M™ Outdoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ .. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M P1500 Medical Permanent Acrylic Adhesives 3M™ Medical Permanent Acrylic Adhesives P1500 demonstrates excellent peel and tack performance and are designed for use in the medical attachment market.Information provided by 3M |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M FM01961K MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Maximum Service Temperature, Air | 49.0 °C | 120 °F | Application |
3M OFL0102 Outdoor UL Recognized Lexan Label Products 3M™ Outdoor UL Recognized Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P.. |