Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Controltac™ 160 Graphic Film 4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Controltac™ 3545C Removable Graphic Film with Comply™ Adhesive 4-mil white, opaque, polyolefin film; Chloride-free film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast and easy application; Remova.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | Curved or corrugated surfaces with rivets |
3M Controltac™ 8620Cv2 ES Changeable Graphic Film with Comply™ v2 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ 3650-10 Graphic Film 2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ 50-12 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ 50-84 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ 8171 Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-10 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-114 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-273 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-37 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-77 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-85 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | Dry, flat surfaces without rivets |
3M Scotchlite™ 5100R Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Pressure-sensitive adhesive; Removable with heat; Available in 15 colors, including black (which ref.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | flat surfaces without rivets |
3M Scotchlite™ 680-14 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | flat surfaces without rivets |
3M Scotchlite™ 680-64 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | flat surfaces without rivets |
3M Scotchlite™ 680-72 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | Curves or corrugations with rivets |
3M Controltac™ IJ180C-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-12 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-22 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-307 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-31 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7125-39 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7725-177 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7725-37 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7725-77 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | flat surfaces without rivets |
3M Scotchlite™ 680-76 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ 8671 Perforated Window Graphic Film Allows a full image to be seen on the outside while allowing viewing through windows from the inside; 4-mil, opaque vinyl film with a high gloss finish; White on the outside facing image side, black.. |
|||
Maximum Service Temperature, Air | 38.0 °C | 100 °F | |
3M Scotchcal™ ElectroCut™ 7725-57 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |