Thermal Properties Metric English Comments
Maximum Service Temperature, Air 5.00 - 70.0 °C
41.0 - 158 °F
SMACTANE®
SMAC SMACMOUNT® 2528S Damping Material
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCou..
Maximum Service Temperature, Air 65.0 - 70.0 °C
149 - 158 °F
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling
Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas..