SMAC SMACMOUNT® 2528S Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACMOUNT®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACMOUNT® 2528S Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Specifications - Shock & vibration insulation for:Aircraft avionics components & subassembliesMissile electronicsVehicular electronics requiring vibration isolationAdvantages :Bushing style mountCountersunk for lowest installed heightCan be pre-loaded to vary natural frequencyAxial to radial stiffness ratio of approx. 1:1Information provided by SMAC MontBlac Groupe Technologies
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 5.00 - 70.0 °C
41.0 - 158 °F
SMACTANE®
-55.0 - 150 °C
-67.0 - 302 °F
SMACSIL®
Descriptive Properties Value Comments
Axial/Radial frequency ratio 1/1 approx.
Frequency 25-40 Hz
Load 0.5 - 3 kg
per isolator
Materials SMACSIL®
SMACTANE®
Maximum axial deflection 8 mm
Metal parts Aluminum and cromated coating
Transmissibility at resonance <2.5
SMACTANE®
<4
SMACSIL®
Weight <60 g