Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 92.0 - 244 °C | 198 - 471 °F | Average value: 148 °C Grade Count:8 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |