Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 97.8 °C | 208 °F | Heat Distortion, Annealed; ASTM D648 |
Total 819E Polystyrene
(discontinued **) Polystyrene 819E is a high impact polystyrene extrusion grade with very high stiffness and thermal properties.It makes an excellent gloss/cut resistant layer for foam applications or general thermof.. |
|||
Maximum Service Temperature, Air | 97.8 °C | 208 °F | Heat Distortion, Annealed; ASTM D648 |
Total 965E Polystyrene
(discontinued **) Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially desig.. |