Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total 965E Polystyrene  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total 965E Polystyrene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polystyrene 965E is a high-impact polystyrene. The extruder will see that 965E produces sheet with a dull matte finish and superior wetting tension to meet the printers needs.965E is specially designed for lithographic printing sheet.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 2.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Elongation at Yield 45 %
45 %
ASTM D638
Tensile Modulus 1.79 GPa
260 ksi
ASTM D638
Flexural Strength 49.6 MPa
7200 psi
ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Falling Dart Impact 9.04 J
6.67 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 97.8 °C
208 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 102 °C
216 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 52 %
52 %
60°; ASTM D523